C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Ti(%) |
---|---|---|---|---|---|---|---|
Max 0.08 | Max 1.0 | Max 1.0 | Max 0.04 | Max 0.030 | 10.5-12.5 | Max 1.0 | 6x%C≤1.0 |
Proof strength Rp0.2(MPa) |
Tensile strength Rm(MPa) |
Impact energy KV(J) |
Elongation at fracture A(%) |
Reduction in cross section on fracture Z(%) |
As-Heat-Treated Condition | Brinell hardness(HBW) |
---|---|---|---|---|---|---|
741(≥) | 526(≥) | 23 | 14 | 44 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 343 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J/kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
596(≥) | 728(≥) | 32 | 44 | 21 | Solution and Aging,Annealing,Ausaging,Q+T,etc | 222 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0)N/mm2 |
Creep rupture strength (10000h) (Rp1,0)N/mm2 |
|||||
856 | 654 | 336 |
Product type | Products | Dimension | Processes | Deliver Status |
---|---|---|---|---|
Plates/Sheets | Plates/Sheets | 0.08-200mm(T)*W*L | Forging,hot rolling and cold rolling | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Steel Bar | Round Bar,Flat Bar,Square Bar | Φ8-1200mm*L | Forging,hot rolling and cold rolling,Cast | Black,Rough Turning,Shot Blasting, |
Coil/Strip | Steel Coil/Steel Strip | 0.03-16.0x1200mm | Cold-Rolled&Hot-Rolled | Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting |
Pipes/Tubes | Seamless Pipes/Tubes,Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion,Cold Drawn,Welded | Annealed,Solution and Aging,Q+T,ACID-WASHED |
Steel grade | Dimension | Shape | Unit | Quantity | Delivery state | Query |
---|---|---|---|---|---|---|
Incoloy800 round bar | Φ115*1400 | Round Bar | Kgs | 169 | Hot-Rolled+Annealed+black | Enquiry |
H13 Tool Steel | 50x710xL | Flat or Square bar | PCS | 4 | Forged+Annealed+black | Enquiry |
1.2344(H13/X40CrMoV5-1/Z40CDV5) Stock List | Dia.182mm - Dia.510mm | Round Bar | Tons | 120 | Forged+Annealed+black | Enquiry |
PH13-8Mo Forgings | Select | 0 | Select | Enquiry | ||
0Cr13Ni8Mo2Al, PH13-8Mo, 13-8Mo, XM-13 round bar stock | Select | 0 | Select | Enquiry |