Lapelloy Stainless Steels to SAE J 467 (1968)

Lapelloy - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of Lapelloy grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.30
Si - 0.25
Mn - 1.00
Ni - 0.30
Cr - 12.00
Al - -
Cu - -
Ti - -
Fe - remaining
Mo - 2.75
Co - -
V - 0.25

Lapelloy - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade Lapelloy SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
294 (≥) 735 (≥) 11 23 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade Lapelloy SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
936 (≥) 549 (≥) 14 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 223
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
492 912 613

Equivalent Products

We can customize the production of Lapelloy grade, contact us for the best solution.