MP35N Superalloys to AMS 5844

MP35N - Specification & Application

  • AMS 5844 -
  • AMS 5845 -
  • ASTM F562 -
  • ISO 15156-3(NACE MR 0175) -
  • ISO 5832-6 -

Medical Devices Marine Engineering

Chemical composition(wt.%) of MP35N grade: to AMS 5844

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
P - 0.015
Si - 0.15
Ni 33.00 37.00
Co - Bal
Mn - 0.15
S - 0.01
Cr 19.00 21.00
Mo 9.00 10.50
Ti - 1.00
Fe - 1.00

MP35N - Detail

MP35N is an age hardenable Nickel-Cobalt base alloy that has a unique combination of properties - ultra high strength, toughness, ductility and outstanding corrosion resistance. MP35N resists corrosion in hydrogen sulphide, salt water and other chloride solutions. It also has excellent resistance to crevice and stress corrosion cracking in sea water and other hostile environments. Suitable where a high combination of strength, high modulus values and good corrosion resistance are required. Applications for this alloy also include medical devices and dental products.

Combination of high strength, ductility and good mechanical properties at ambient temperatures Excellent corrosion resistance in hydrogen sulphide Excellent resistance to crevice and stress corrosion cracking in sea water Age hardenable (Spring Temper only)

Mechanical properties of grade MP35N AMS 5844

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
551 (≥) 528 (≥) 44 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 441

Physical properties of grade MP35N AMS 5844

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
763 (≥) 737 (≥) 13 43 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
299 881 216

Equivalent Grade

Equivalent Products

We can customize the production of MP35N grade, contact us for the best solution.