N07080 Stainless Steels

N07080 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of N07080 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 1.00
Mn - 1.00
P - 0.045
S - 0.030
Cr 18.0 21.0
Ni - remaining

N07080 - Detail

Steel for exhaust valves

Mechanical properties of grade N07080

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
549 (≥) 289 (≥) 31 13 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 342

Physical properties of grade N07080

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
236 (≥) 712 (≥) 42 13 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
425 455 696

Equivalent Grade

We can customize the production of N07080 grade, contact us for the best solution.