N07751 Stainless Steels

N07751 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of N07751 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.03 0.10
Si - 0.50
Mn - 0.50
P - 0.015
S - 0.015
Cr 14.0 17.0
Ni - remaining
Mo - 0.50

N07751 - Detail

Steel for exhaust valves

Mechanical properties of grade N07751

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
183 (≥) 571 (≥) 24 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade N07751

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
396 (≥) 221 (≥) 13 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
817 264 157