N08028 Stainless Steels

N08028 - Specification & Application

Ni-Fe-Cr Alloy Solid Solution Strengthened

Chemical composition(wt.%) of N08028 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn - 2.00
Si - 1.00
P - 0.02
S - 0.015
Cr 26.00 28.00
Ni 29.50 32.50
Mo 3.00 4.00
Cu 0.60 1.40

N08028 - Detail

Ni-Fe-Cr Alloy Solid Solution Strengthened

Mechanical properties of grade N08028

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
965 (≥) 614 (≥) 34 22 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade N08028

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
387 (≥) 228 (≥) 41 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
116 638 341
We can customize the production of N08028 grade, contact us for the best solution.