NC15Fe7TA Stainless Steels to NF A 35-579

NC15Fe7TA - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of NC15Fe7TA grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.80
Si - 0.50
Mn - 1.00
P - 0.015
S - 0.015
Cr 14.00 17.00
Ni - remaining
Mo - 0.50
Fe 5.00 9.00
Al 0.40 1.00
Ti 2.25 2.75
Nb+Ta 0.70 1.20
Co - 1.00
Cu - 0.50

NC15Fe7TA - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade NC15Fe7TA NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
123 (≥) 245 (≥) 21 41 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade NC15Fe7TA NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
588 (≥) 669 (≥) 23 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
538 329 573

Equivalent Grade

Equivalent Products

We can customize the production of NC15Fe7TA grade, contact us for the best solution.