Chemical composition(wt.%) of NCF 750 grade: to G 4902 (1991)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.50
Mn - 1.00
P - 0.03
S - 0.015
Cr 14.00 17.00
Ni 70.00 -
Cu - 0.50
Al 0.40 1.00
Ti 2.25 2.75
Fe 5.00 9.00
Nb+Ta 0.70 1.20

NCF 750 - Detail

Corrosion-resisting and heat-resisting superalloy plates and sheets

Mechanical properties of grade NCF 750 G 4902 (1991)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
863 (≥) 879 (≥) 32 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade NCF 750 G 4902 (1991)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
622 (≥) 448 (≥) 31 43 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
413 327 643