Chemical composition(wt.%) of NCF80A grade: to D 3531 (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 1.00
P - 0.030
S - 0.015
Cr 18.00 21.00
Ni - remaining
Cu - 0.20
Al 1.00 1.80
Ti 1.80 2.20
Fe - -

NCF80A - Detail

Corrosion - resisting and heat - resisting superalloy plates and sheets

Mechanical properties of grade NCF80A D 3531 (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
431 (≥) 859 (≥) 44 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade NCF80A D 3531 (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
372 (≥) 323 (≥) 21 22 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
755 919 776