Chemical composition(wt.%) of P20 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.28 0.40
Si 0.20 0.80
Mn 0.60 1.00
P - 0.030
S - 0.030
Cr 1.40 2.00
Mo 0.30 0.55
V - -
W - -
Ni+Cu - 0.75

P20 - Detail

Mold Steel

Mechanical properties of grade P20

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
981 (≥) 146 (≥) 34 21 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade P20

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
534 (≥) 864 (≥) 41 13 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
161 239 274