R30783 Stainless Steels

R30783 - Specification & Application

Co-Ni-Fe-Al-Nb-Cr alloy

Chemical composition(wt.%) of R30783 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn 3.75 4.75
P - 0.045
S - 0.03
Ni 9.00 10.50
Cr 19.00 22.00
Al - -
Cu - -
Ti - -
Fe - -
N - -
Mo - -
V - -

R30783 - Detail

Co-Ni-Fe-Al-Nb-Cr alloy

Mechanical properties of grade R30783

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
342 (≥) 639 (≥) 31 11 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade R30783

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
846 (≥) 325 (≥) 34 44 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
916 392 989
We can customize the production of R30783 grade, contact us for the best solution.