S2 Tool Die Steels

S2 - Specification & Application

Shock-Resisting Tool Steel

Chemical composition(wt.%) of S2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.40 0.55
Si 0.90 1.20
Mn 0.30 0.50
P - 0.030
S - 0.030
Cr - -
Mo 0.30 0.60
V - 0.50
W - -
Ni+Cu - 0.75

S2 - Detail

Shock-Resisting Tool Steel

Mechanical properties of grade S2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
292 (≥) 476 (≥) 22 21 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade S2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
476 (≥) 558 (≥) 22 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
359 665 475
We can customize the production of S2 grade, contact us for the best solution.