S20161 Stainless Steels

S20161 - Specification & Application

Austenitic Chromium Manganese Nickel Silicon Stainless Steel

Chemical composition(wt.%) of S20161 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 3.00 4.00
Mn 4.00 6.00
P - 0.04
S - 0.04
Cr 15.0 18.0
Ni 4.00 6.00
N 0.08 0.20

S20161 - Detail

S20161

Mechanical properties of grade S20161

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
717 (≥) 233 (≥) 42 12 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade S20161

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
846 (≥) 588 (≥) 33 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
879 384 369

Equivalent Products