S21603 Stainless Steels

S21603 - Specification & Application

Austenitic Chromium Manganese Nickel Molybdenum Stainless Steel

Chemical composition(wt.%) of S21603 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn 7.50 9.00
P - 0.045
S - 0.03
Cr 17.5 22.0
Ni 5.00 7.00
Mo 2.00 3.00
N 0.25 0.50

S21603 - Detail

S21603

Mechanical properties of grade S21603

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
998 (≥) 276 (≥) 24 33 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade S21603

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
932 (≥) 665 (≥) 21 21 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
698 449 224

Equivalent Products

We can customize the production of S21603 grade, contact us for the best solution.