S41026 Stainless Steels

S41026 - Specification & Application

Martensitic Chromium Stainless Steel with Molybdenum

Chemical composition(wt.%) of S41026 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn - 1.00
Si - 1.00
P - 0.02
S - 0.02
Cr 11.50 13.50
Ni 1.00 2.00
Mo 0.40 0.60
Cu - 0.50

S41026 - Detail

Martensitic Chromium Stainless Steel with Molybdenum

Mechanical properties of grade S41026

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
936 (≥) 891 (≥) 31 32 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade S41026

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
242 (≥) 169 (≥) 34 42 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
892 548 873