S44002 Stainless Steels

S44002 - Specification & Application

Hardenable Chromium Stainless Steel

Chemical composition(wt.%) of S44002 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.60 0.75
Mn - 1.00
Si - 1.00
P - 0.04
S - 0.03
Cr 16.00 18.00
Ni - -
Mo - 0.75

S44002 - Detail

Hardenable Chromium Stainless Steel

Mechanical properties of grade S44002

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
931 (≥) 657 (≥) 42 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade S44002

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
148 (≥) 336 (≥) 24 41 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
492 296 854
We can customize the production of S44002 grade, contact us for the best solution.