S44625 Stainless Steels

S44625 - Specification & Application

Low Interstitial Ferritic Chromium Stainless Steel

Chemical composition(wt.%) of S44625 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 0.40
Si - 0.40
P - 0.02
S - 0.02
Cr 25.00 27.00
Ni - 0.50
Mo 0.75 1.50
N - 0.015
Cu 0.20 -

S44625 - Detail

Low Interstitial Ferritic Chromium Stainless Steel

Mechanical properties of grade S44625

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
773 (≥) 876 (≥) 43 24 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade S44625

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
874 (≥) 329 (≥) 11 12 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 221
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
226 797 868

Equivalent Products

We can customize the production of S44625 grade, contact us for the best solution.