SA-693 S13800 Stainless Steels to SA-693

SA-693 S13800 - Specification & Application

  • SA-693 - Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of SA-693 S13800 grade: to SA-693

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Mn - 0.20
Si - 0.10
P - 0.01
S - 0.008
Cr 12.25 13.00
Ni 7.50 8.50
Mo 2.00 2.50
Al 0.90 1.35
N - 0.01

SA-693 S13800 - Detail

Specification for Precipitation-Hardening Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

Mechanical properties of grade SA-693 S13800 SA-693

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
356 (≥) 641 (≥) 43 32 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade SA-693 S13800 SA-693

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
864 (≥) 972 (≥) 31 44 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
613 236 179
We can customize the production of SA-693 S13800 grade, contact us for the best solution.