STS302B Stainless Steels to D 3698 (2008)

STS302B - Specification & Application

  • D 3698 (2008) - Cold rolled stainless steel plates, sheets and strip
  • D 3705 (2008) - Hot rolled stainless steel plates, sheets and strip

Hot rolled stainless steel plates, sheets and strip

Chemical composition(wt.%) of STS302B grade: to D 3698 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si 2.00 3.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 17.00 19.00
Ni 8.00 10.00
Mo - -
N - -

STS302B - Detail

Hot rolled stainless steel plates, sheets and strip

Mechanical properties of grade STS302B D 3698 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
161 (≥) 196 (≥) 43 42 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade STS302B D 3698 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
898 (≥) 391 (≥) 12 41 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
763 574 849

Equivalent Grade

Equivalent Products

We can customize the production of STS302B grade, contact us for the best solution.
sales@specificsteel.com