Chemical composition(wt.%) of STS631J1 grade: to D 3535 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 16.00 18.00
Ni 7.00 8.50
Al 0.75 1.50

STS631J1 - Detail

Stainless steel wire rods

Mechanical properties of grade STS631J1 D 3535 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
678 (≥) 465 (≥) 34 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade STS631J1 D 3535 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
812 (≥) 136 (≥) 32 41 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
589 256 556