SUS 420F Stainless Steels to G 4303 (2012)

SUS 420F - Specification & Application

  • G 4303 (2012) - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of SUS 420F grade: to G 4303 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.26 0.40
Si - 1.00
Mn - 1.00
P - 0.06
S - 0.15
Cr 12.00 14.00
Ni - 0.60
Mo - 0.60
N - -

SUS 420F - Detail

Stainless steel bars

Mechanical properties of grade SUS 420F G 4303 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
522 (≥) 237 (≥) 34 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade SUS 420F G 4303 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
543 (≥) 363 (≥) 14 44 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
848 716 166

Equivalent Products

We can customize the production of SUS 420F grade, contact us for the best solution.