SUS 440C Stainless Steels to G 4309 (1999)

SUS 440C - Specification & Application

  • G 4309 (1999) - Stainless steel wires

Stainless steel wires

Chemical composition(wt.%) of SUS 440C grade: to G 4309 (1999)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.20
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 16.00 18.00
Ni - 0.60
Mo - 0.75
N - -

SUS 440C - Detail

Stainless steel wires

Mechanical properties of grade SUS 440C G 4309 (1999)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
578 (≥) 439 (≥) 23 34 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade SUS 440C G 4309 (1999)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
392 (≥) 681 (≥) 32 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
993 789 517