Stellite 12P Tool Die Steels

Stellite 12P - Specification & Application

Stellite alloy

Chemical composition(wt.%) of Stellite 12P grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 1.40
Si - -
Mn - -
Cr - 31.00
Ni - -
Mo - -
Co remaining -
W - 9.00
Fe - -

Stellite 12P - Detail

Stellite alloy

Mechanical properties of grade Stellite 12P

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
478 (≥) 153 (≥) 34 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade Stellite 12P

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
522 (≥) 277 (≥) 14 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 242
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
483 412 346

Equivalent Grade

Equivalent Products

We can customize the production of Stellite 12P grade, contact us for the best solution.