Stellite 30 Tool Die Steels

Stellite 30 - Specification & Application

Stellite alloy

Chemical composition(wt.%) of Stellite 30 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.45
Si - 0.60
Mn - 0.60
Cr - 26.00
Ni - 15.00
Mo - 6.00
Co remaining -
W - -
Fe - 1.00

Stellite 30 - Detail

Stellite alloy

Mechanical properties of grade Stellite 30

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
362 (≥) 433 (≥) 14 22 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade Stellite 30

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
481 (≥) 136 (≥) 32 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 432
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
711 453 849

Equivalent Grade

Equivalent Products

We can customize the production of Stellite 30 grade, contact us for the best solution.