T12001 Tool Die Steels

T12001 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of T12001 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.65 0.80
Si 0.20 0.40
Mn 0.10 0.40
P - 0.030
S - 0.030
Cr 3.75 4.50
Mo - -
V 0.90 1.30
W 17.25 18.75
Co - -

T12001 - Detail

High-Speed Tool Steel

Mechanical properties of grade T12001

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
564 (≥) 977 (≥) 11 22 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade T12001

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
959 (≥) 392 (≥) 13 33 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
877 521 177

Equivalent Grade

Equivalent Products

We can customize the production of T12001 grade, contact us for the best solution.