High-Speed Tool Steel
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.75 | 0.85 | ||
Si | 0.20 | 0.40 | ||
Mn | 0.20 | 0.40 | ||
P | - | 0.030 | ||
S | - | 0.030 | ||
Cr | 3.75 | 5.00 | ||
Mo | 0.50 | 1.25 | ||
V | 1.80 | 2.40 | ||
W | 17.50 | 19.00 | ||
Co | 7.00 | 9.50 |
High-Speed Tool Steel
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
514 (≥) | 357 (≥) | 31 | 11 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 213 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
368 (≥) | 797 (≥) | 22 | 12 | 32 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 442 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
339 | 862 | 968 |
We can customize the production of T12005 grade, contact us for the best solution.