T201LN Stainless Steels

T201LN - Specification & Application

Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of T201LN grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn 6.40 7.50
P - 0.045
S - 0.015
Cr 16.0 17.5
Ni 4.00 5.00
N 0.10 0.25
Cu - 1.00

T201LN - Detail

T201LN

Mechanical properties of grade T201LN

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
384 (≥) 351 (≥) 12 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade T201LN

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
144 (≥) 847 (≥) 22 11 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
149 825 335

Equivalent Grade

Equivalent Products