T20811 Tool Die Steels

T20811 - Specification & Application

Hot-Work Tool Steel

Chemical composition(wt.%) of T20811 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.33 0.43
Si 0.80 1.20
Mn 0.20 0.50
P - 0.030
S - 0.030
Cr 4.75 5.50
Mo 1.10 1.60
V 0.30 0.60
W - -
Ni+Cu - 0.75

T20811 - Detail

Hot-Work Tool Steel

Mechanical properties of grade T20811

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
526 (≥) 766 (≥) 31 22 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade T20811

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
489 (≥) 989 (≥) 22 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
538 951 977

Equivalent Grade

Equivalent Products

We can customize the production of T20811 grade, contact us for the best solution.