T30105 Tool Die Steels

T30105 - Specification & Application

Cold-Work Tool Steel

Chemical composition(wt.%) of T30105 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.95 1.05
Si 0.10 0.50
Mn 2.80 3.20
P - 0.030
S - 0.030
Cr 0.90 1.20
Mo 0.90 1.40
V - -
W - -
Ni+Cu - 0.75

T30105 - Detail

Cold-Work Tool Steel

Mechanical properties of grade T30105

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
738 (≥) 259 (≥) 12 23 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade T30105

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
595 (≥) 146 (≥) 43 42 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
433 926 548

Equivalent Grade

Equivalent Products