T30405 Tool Die Steels

T30405 - Specification & Application

Cold-Work Tool Steel

Chemical composition(wt.%) of T30405 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 1.40 1.60
Si 0.10 0.60
Mn 0.20 0.60
P - 0.030
S - 0.030
Cr 11.00 13.00
Mo 0.70 1.20
V - 1.00
W - -
Ni+Cu - 0.75
Co 2.50 3.50

T30405 - Detail

Cold-Work Tool Steel

Mechanical properties of grade T30405

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
286 (≥) 237 (≥) 32 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade T30405

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
836 (≥) 721 (≥) 14 13 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 421
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
259 498 973

Equivalent Grade

Equivalent Products