W12Cr4V5Co5 Special Alloy

Chemical composition%of the ladle analysis of gradeW12Cr4V5Co5

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Mo(%)V(%)W(%)Co(%)
1.50~1.600.15~0.400.15~0.40≤0.030≤0.0303.75~5.00<1.004.50~5.2511.75~13.004.75~5.25
The performance characteristics of high-speed tool steel with purpose

(1) use of steel DianZhaLu smelting, the silicon content not specified limit.
(2) in order to improve steel cutting machining, the buyer's request, can be provisions for sulfur ω (S) 0.60% ~ 0.15%.
(3) of residual elements in steel (mass fraction) : 0.30% or Ni; Cu 0.25% or less.
(4) is the high tungsten molybdenum content allowed ω (Mo) more than 1.00%. Steel tungsten molybdenum and the relationship is: when molybdenum content more than ω (Mo) 0.30%, tungsten content reduced correspondingly, in molybdenum content more than ω (Mo) 0.30% of the part, each ω (Mo) 1% can replace ω (W) 2%, if meet this kind of case, in this GangHao add after "Mo".
(5) W6Mo5Cr4V2 steel according to both the supply and the demand agreement, adjust the content of vanadium ω (V) 1.60% ~ 2.20%.

Mechanical properties of gradeW12Cr4V5Co5

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
845(≥) 691(≥) 23 34 22 Solution and Aging,Annealing,Ausaging,Q+T,etc 313

Physical properties of grade W12Cr4V5Co5

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
336(≥) 913(≥) 12 34 14 Solution and Aging,Annealing,Ausaging,Q+T,etc 312
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
298 522 616

W12Cr4V5Co5 Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Grade