Waspaloy Stainless Steels to SAE AMS 5544J (2008)

Waspaloy - Specification & Application

  • SAE AMS 5544J (2008) - Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted, Annealed

Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted, Annealed

Chemical composition(wt.%) of Waspaloy grade: to SAE AMS 5544J (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 0.10
Mn - 0.10
Cr - 19.75
Ni - remaining
Mo - 4.45
Co - 14.00
W - -
Al - 1.40
Cu - -
Ti - 3.00
Fe - 0.75
B - 0.005
Zr - 0.04

Waspaloy - Detail

Nickel Alloy, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 57Ni - 19.5Cr - 13.5Co - 4.2Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted, Annealed

Mechanical properties of grade Waspaloy SAE AMS 5544J (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
913 (≥) 831 (≥) 23 32 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade Waspaloy SAE AMS 5544J (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
814 (≥) 394 (≥) 43 11 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
963 569 724

Equivalent Products

We can customize the production of Waspaloy grade, contact us for the best solution.