X 19 CrMoNbVN 11-1 Stainless Steels to DIN EN 10088-1

X 19 CrMoNbVN 11-1 - Specification & Application

  • DIN EN 10088-1 - Stainless steels - Part 1: list of stainless steels
  • DIN EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties
  • DIN EN 10302 (2002) - Creep resisting steels, nickel and cobalt alloys

Stainless steels - Part 1: list of stainless steels

Chemical composition(wt.%) of X 19 CrMoNbVN 11-1 grade: to DIN EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.1700 0.2300
Mn 0.4000 0.9000
P - 0.0250
S - 0.0150
Si - 0.5000
Ni 0.2000 0.6000
Cr 10.0000 11.5000
Mo 0.5000 0.8000
V 0.1000 0.3000
B - 0.0015
Al - 0.0200
N 0.0500 0.1000
Nb 0.2500 0.5500

X 19 CrMoNbVN 11-1 - Detail

Stainless steels - Part 1: list of stainless steels

Mechanical properties of grade X 19 CrMoNbVN 11-1 DIN EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
611 (≥) 746 (≥) 21 41 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 113

Physical properties of grade X 19 CrMoNbVN 11-1 DIN EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
141 (≥) 834 (≥) 21 32 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
553 995 492

Equivalent Products