X10CrAlSi25 Stainless Steels to ISO 15510 (2010)

X10CrAlSi25 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 4955 (2005) - Heat-resistant steels

Heat-resistant steels

Chemical composition(wt.%) of X10CrAlSi25 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si 0.70 1.40
Mn - 1.00
P - 0.040
S - 0.030
Cr 23.00 26.00
Ni - 1.00
Al 0.70 1.20

X10CrAlSi25 - Detail

Heat-resistant steels

Mechanical properties of grade X10CrAlSi25 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
529 (≥) 225 (≥) 42 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade X10CrAlSi25 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
589 (≥) 691 (≥) 21 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 114
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
229 585 178

Equivalent Products

We can customize the production of X10CrAlSi25 grade, contact us for the best solution.