X12Cr13 Stainless Steels to ISO 15510 (2010)

X12Cr13 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 16143-1 (2004) - Stainless steels for general purposes -- Part 1: Flat products
  • ISO 16143-2 (2004) - Stainless steels for general purposes -- Part 2: Semi-finished products, bars, rods and sections
  • ISO 16143-3 (2005) - Stainless steels for general purposes -- Part 3: Wire
  • ISO/TR 4956 - Wrought steels for use at elevated temperatures in engines
  • ISO/TS 15510 (2003) - Stainless steels - Chemical composition

Stainless steels - Chemical composition

Chemical composition(wt.%) of X12Cr13 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 1.00
Mn - 1.50
P - 0.040
S - 0.030
Cr 11.50 13.50
Ni - 0.75
Mo - -
N - -

X12Cr13 - Detail

Stainless steels - Chemical composition

Mechanical properties of grade X12Cr13 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
712 (≥) 373 (≥) 23 24 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade X12Cr13 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
743 (≥) 554 (≥) 24 31 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 143
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
785 828 374

Equivalent Products