X1CrNiMoCuN25-25-5 Stainless Steels to BS EN 10028-7

X1CrNiMoCuN25-25-5 - Specification & Application

  • BS EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
  • BS EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Chemical composition(wt.%) of X1CrNiMoCuN25-25-5 grade: to BS EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Si - 0.70
Mn - 2.00
P - 0.03
S - 0.01
Cr 24.00 26.00
Ni 24.00 27.00
Mo 4.70 5.70
N 0.17 0.25
Cu 1.00 2.00

X1CrNiMoCuN25-25-5 - Detail

Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Mechanical properties of grade X1CrNiMoCuN25-25-5 BS EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
858 (≥) 225 (≥) 12 43 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade X1CrNiMoCuN25-25-5 BS EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
747 (≥) 157 (≥) 24 43 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
137 581 159

Equivalent Products

We can customize the production of X1CrNiMoCuN25-25-5 grade, contact us for the best solution.
sales@specificsteel.com