X22CrMoV12-1 Stainless Steels to NF EN 10088-1

X22CrMoV12-1 - Specification & Application

  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties
  • NF EN 10302 (2002) - Creep resisting steels, nickel and cobalt alloys

Creep resisting steels, nickel and cobalt alloys

Chemical composition(wt.%) of X22CrMoV12-1 grade: to NF EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.18 0.24
Si - 0.50
Mn 0.40 0.90
P - 0.025
S - 0.015
Cr 11.00 12.50
Ni 0.30 0.80
Mo 0.80 1.20
V 0.25 0.35

X22CrMoV12-1 - Detail

Creep resisting steels, nickel and cobalt alloys

Mechanical properties of grade X22CrMoV12-1 NF EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
195 (≥) 497 (≥) 33 21 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade X22CrMoV12-1 NF EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
383 (≥) 966 (≥) 22 13 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
614 685 165