X2CrNiMoN17-11-2 Stainless Steels to DIN EN 10088-1

X2CrNiMoN17-11-2 - Specification & Application

  • DIN EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • DIN EN 10088-2 - Stainless steels - Part 2: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
  • DIN EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • DIN EN 10088-4 - Stainless steels - Part 4: Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes
  • DIN EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes
  • DIN 17440 (1975) - Stainless steels - Technical delivery conditions for drawn wire
  • DIN 17441 (1997) - Stainless steels - Technical delivery conditions for cold rolled strips and slit coils strip and sheets cut from such strips for pressure purposes
  • DIN 17440 (1996) - Stainless steels - Technical delivery conditions for drawn wire
  • DIN EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • DIN EN 10222-5 - Steel forgings for pressure purposes - Part 5: Martensitic, austenitic and austenitic-ferritic stainless steels
  • DIN EN 10250-4 - Open die steel forgings for general engineering purposes - Part 4: Stainless steels
  • DIN EN 10272 - Stainless steel bars for pressure purposes

DIN 1654-5 (1989) Cold heading and cold extruding steels; technical delivery conditions for stainless steels; Replaced by DIN EN 10263-5:2002

Chemical composition(wt.%) of X2CrNiMoN17-11-2 grade: to DIN EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 16.5 18.5
Mo 2.00 2.50
Ni 10.0 12.0
N 0.12 0.22

X2CrNiMoN17-11-2 - Detail

DIN 1654-5 (1989) Cold heading and cold extruding steels; technical delivery conditions for stainless steels; Replaced by DIN EN 10263-5:2002

Mechanical properties of grade X2CrNiMoN17-11-2 DIN EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
747 (≥) 933 (≥) 31 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade X2CrNiMoN17-11-2 DIN EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
496 (≥) 673 (≥) 41 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
355 319 837

Equivalent Products

We can customize the production of X2CrNiMoN17-11-2 grade, contact us for the best solution.
sales@specificsteel.com