X2CrNiMoN22-5-3 Stainless Steels to ISO 15510 (2010)

X2CrNiMoN22-5-3 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 16143-1 (2004) - Stainless steels for general purposes -- Part 1: Flat products
  • ISO 16143-2 (2004) - Stainless steels for general purposes -- Part 2: Semi-finished products, bars, rods and sections
  • ISO 16143-3 (2005) - Stainless steels for general purposes -- Part 3: Wire
  • ISO 9327-5 (1999) - Steel forgings and rolled or forged bars for pressure purposes - Technical delivery conditions - Part 5: Stainless steels
  • ISO 9328-7 (2011) - Steel flat products for pressure purposes - Technical delivery conditions - Part 7: Stainless steels
  • ISO/TS 15510 (2003) - Stainless steels - Chemical composition

Stainless steels - Chemical composition

Chemical composition(wt.%) of X2CrNiMoN22-5-3 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.015
Cr 21.00 23.00
Ni 4.50 6.50
Mo 2.50 3.50
N 0.10 0.22

X2CrNiMoN22-5-3 - Detail

Stainless steels - Chemical composition

Mechanical properties of grade X2CrNiMoN22-5-3 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
217 (≥) 291 (≥) 11 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade X2CrNiMoN22-5-3 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
394 (≥) 723 (≥) 33 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
362 264 148

Equivalent Products

We can customize the production of X2CrNiMoN22-5-3 grade, contact us for the best solution.