X2CrTi12 Stainless Steels to ISO 15510 (2010)

X2CrTi12 - Specification & Application

  • ISO 15510 (2010) - Stainless steels -- Chemical composition
  • ISO 16143-1 (2004) - Stainless steels for general purposes -- Part 1: Flat products
  • ISO 4955 (2005) - Heat-resistant steels
  • ISO/TS 15510 (2003) - Stainless steels - Chemical composition

Stainless steels - Chemical composition

Chemical composition(wt.%) of X2CrTi12 grade: to ISO 15510 (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 10.50 12.50
Ni - 0.50
Mo - -
N - -
Ti 6×(C+N)% 0.65

X2CrTi12 - Detail

Stainless steels - Chemical composition

Mechanical properties of grade X2CrTi12 ISO 15510 (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
594 (≥) 317 (≥) 11 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade X2CrTi12 ISO 15510 (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
676 (≥) 476 (≥) 21 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
885 523 414