X3CrNi13-4 Stainless Steels to DIN 17145 (1980)

X3CrNi13-4 - Specification & Application

  • DIN 17145 (1980) - Round Wire Rod for Welding Filler Metals; Technical Conditions of Delivery

Round Wire Rod for Welding Filler Metals; Technical Conditions of Delivery

Chemical composition(wt.%) of X3CrNi13-4 grade: to DIN 17145 (1980)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.70
Mn - 1.50
P - 0.040
S - 0.015
Cr 12.0 14.0
Mo 0.30 0.70
Ni 3.50 4.50
N - 0.020

X3CrNi13-4 - Detail

Round Wire Rod for Welding Filler Metals; Technical Conditions of Delivery

Mechanical properties of grade X3CrNi13-4 DIN 17145 (1980)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
181 (≥) 374 (≥) 44 14 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade X3CrNi13-4 DIN 17145 (1980)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
278 (≥) 364 (≥) 43 31 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 314
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
761 834 589

Equivalent Products

We can customize the production of X3CrNi13-4 grade, contact us for the best solution.