X3CrNiMoBN17-13-3 Stainless Steels to NF EN 10028-7

X3CrNiMoBN17-13-3 - Specification & Application

  • NF EN 10028-7 - Flat products made of steels for pressure purposes - Part 7: Stainless steels
  • NF EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • NF EN 10216-5 (2004) - Seamless steel tubes for pressure purposes - Technical delivery conditions - Part 5: Stainless steel tubes
  • NF EN 10222-5 - Steel forgings for pressure purposes - Part 5: Martensitic, austenitic and austenitic-ferritic stainless steels
  • NF EN 10269 - Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties
  • NF EN 10302 (2002) - Creep resisting steels, nickel and cobalt alloys

Creep resisting steels, nickel and cobalt alloys

Chemical composition(wt.%) of X3CrNiMoBN17-13-3 grade: to NF EN 10028-7

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.040
Si - 0.75
Mn - 2.00
P - 0.035
S - 0.015
Cr 16.00 18.00
Ni 12.00 14.00
Mo 2.00 3.00
N 0.10 0.18
B 0.0015 0.0050

X3CrNiMoBN17-13-3 - Detail

Creep resisting steels, nickel and cobalt alloys

Mechanical properties of grade X3CrNiMoBN17-13-3 NF EN 10028-7

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
677 (≥) 387 (≥) 43 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade X3CrNiMoBN17-13-3 NF EN 10028-7

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
414 (≥) 742 (≥) 41 11 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
961 372 334

Equivalent Products

We can customize the production of X3CrNiMoBN17-13-3 grade, contact us for the best solution.
sales@specificsteel.com