X5CrNiMo17-12 2E Stainless Steels to ISO 4954

X5CrNiMo17-12 2E - Specification & Application

  • ISO 4954 - Steels for cold heading and cold extruding

Steels for cold heading and cold extruding

Chemical composition(wt.%) of X5CrNiMo17-12 2E grade: to ISO 4954

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.07
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.030
Cr 16.50 18.50
Ni 10.50 13.50
Mo 2.00 2.50

X5CrNiMo17-12 2E - Detail

Steels for cold heading and cold extruding

Mechanical properties of grade X5CrNiMo17-12 2E ISO 4954

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
866 (≥) 887 (≥) 23 11 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade X5CrNiMo17-12 2E ISO 4954

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
735 (≥) 169 (≥) 13 31 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
283 515 814

Equivalent Products

We can customize the production of X5CrNiMo17-12 2E grade, contact us for the best solution.