X85CrMoV18-2 Stainless Steels to NF EN 10090

X85CrMoV18-2 - Specification & Application

  • NF EN 10090 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of X85CrMoV18-2 grade: to NF EN 10090

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.80 0.90
Si - 1.50
Mn - 1.50
P - 0.040
S - 0.030
Cr 16.50 18.50
Ni - -
Mo 2.00 2.50
V 0.30 0.60

X85CrMoV18-2 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade X85CrMoV18-2 NF EN 10090

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
586 (≥) 655 (≥) 22 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade X85CrMoV18-2 NF EN 10090

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
491 (≥) 162 (≥) 24 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
213 381 495