XH62MBKЮ Special Alloy

Chemical composition%of the ladle analysis of gradeXH62MBKЮ

C(%)Si(%)Mn(%)P(%)S(%)Cr(%)Ni(%)Mo(%)W(%)Co(%)B(%)Al(%)Other(%)
Max 0.10Max 0.60Max 0.300.0150.018.5-10.5Balance9.00-11.54.3-6.004.00-6.00Max 0.024.20-4.90Ce: Max 0.02
XH62MBKЮ

Mechanical properties of gradeXH62MBKЮ

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
366(≥) 747(≥) 42 34 21 Solution and Aging,Annealing,Ausaging,Q+T,etc 432

Physical properties of grade XH62MBKЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
798(≥) 867(≥) 11 34 31 Solution and Aging,Annealing,Ausaging,Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
499 421 259

XH62MBKЮ Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED