XH75MБTЮ Stainless Steels

XH75MБTЮ - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH75MБTЮ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.80
Mn - 0.40
P - 0.020
S - 0.012
Cr 19.00 22.00
Ni - remaining
Mo 1.80 2.30
Al 0.35 0.75
Ti 0.35 0.75
Fe - 3.00
Nb 0.90 1.30

XH75MБTЮ - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH75MБTЮ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
152 (≥) 195 (≥) 43 14 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade XH75MБTЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
393 (≥) 735 (≥) 13 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 244
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
213 138 912

Equivalent Grade

Equivalent Products

We can customize the production of XH75MБTЮ grade, contact us for the best solution.