Z 3 CND 17-11-02 Stainless Steels to NF A 35-573

Z 3 CND 17-11-02 - Specification & Application

  • NF A 35-573 - Stainless steels for general purposes. Plates, wide strips and strips
  • NF A 35-574 - Iron and steel. Stainless steel for general purposes. Semi- finished products, bars and wire rod
  • NF A 36-209 - Iron and steel. Austenitic and austenic-ferritic stainless steels plates for boilers and pressure vessels
  • NF A 49-244 - Steel tubes - Welded austenitic stainless and austenitic ferritic steel rolled tubes for pressure service - Dimensions, technical conditions for delivery
  • NF E 29-043 - Non alloy and alloy steel bolting for pressure equipement - Specifications

Austenitic stainless steel. Grade 00Cr17Ni14Mo2 was replaced by new designation 022Cr17Ni12Mo2 according to GB/T 20878 (2007)

Chemical composition(wt.%) of Z 3 CND 17-11-02 grade: to NF A 35-573

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn - 2.00
P - 0.035
S - 0.030
Ni 12.00 15.00
Cr 16.00 18.00
Mo 2.00 3.00

Z 3 CND 17-11-02 - Detail

Stainless and heat resisting steels

Mechanical properties of grade Z 3 CND 17-11-02 NF A 35-573

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
188 (≥) 319 (≥) 11 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade Z 3 CND 17-11-02 NF A 35-573

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
494 (≥) 471 (≥) 31 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
183 423 175

Equivalent Products

We can customize the production of Z 3 CND 17-11-02 grade, contact us for the best solution.