Z12CKNDWNb21-20-20 Stainless Steels to NF A 35-579

Z12CKNDWNb21-20-20 - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of Z12CKNDWNb21-20-20 grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.16
Si - 1.00
Mn 1.00 2.00
P - 0.040
S - 0.030
Cr 20.00 22.50
Ni 19.00 21.00
Mo 2.50 3.50
Co 18.50 21.00
W 2.00 3.00
Nb 0.75 1.25
N 0.10 0.20

Z12CKNDWNb21-20-20 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade Z12CKNDWNb21-20-20 NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
821 (≥) 454 (≥) 23 22 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 244

Physical properties of grade Z12CKNDWNb21-20-20 NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
485 (≥) 145 (≥) 34 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
883 687 227

Equivalent Products

We can customize the production of Z12CKNDWNb21-20-20 grade, contact us for the best solution.