Z12CNDV12-03 Stainless Steels to NF A 35-578

Z12CNDV12-03 - Specification & Application

  • NF A 35-578 - Iron and steel. Stainless steel for high temperature application

Iron and steel. Stainless steel for high temperature application

Chemical composition(wt.%) of Z12CNDV12-03 grade: to NF A 35-578

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 0.35
Mn 0.50 0.90
P - 0.035
S - 0.015
Cr 11.00 12.50
Mo 2.00 3.00
Ni 1.50 2.00
V 0.25 0.40
N 0.020 0.040

Z12CNDV12-03 - Detail

Iron and steel. Stainless steel for high temperature application

Mechanical properties of grade Z12CNDV12-03 NF A 35-578

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
497 (≥) 416 (≥) 41 42 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 234

Physical properties of grade Z12CNDV12-03 NF A 35-578

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
425 (≥) 976 (≥) 23 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
489 431 576

Equivalent Products

We can customize the production of Z12CNDV12-03 grade, contact us for the best solution.