Z35CNWS14-14 Stainless Steels to NF A 35-579

Z35CNWS14-14 - Specification & Application

  • NF A 35-579 - Valve steels and alloys for internal combustion engines

Valve steels and alloys for internal combustion engines

Chemical composition(wt.%) of Z35CNWS14-14 grade: to NF A 35-579

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.30 0.40
Si 1.00 2.00
Mn - 1.00
P - 0.040
S - 0.030
Cr 13.00 15.00
Ni 13.00 15.00
Mo - -
W 2.00 3.00

Z35CNWS14-14 - Detail

Valve steels and alloys for internal combustion engines

Mechanical properties of grade Z35CNWS14-14 NF A 35-579

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
631 (≥) 624 (≥) 14 22 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade Z35CNWS14-14 NF A 35-579

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
548 (≥) 299 (≥) 33 21 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 433
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
224 128 951

Equivalent Grade

Equivalent Products

We can customize the production of Z35CNWS14-14 grade, contact us for the best solution.